3D surface analysis at the nanometre scale –
Non-contact, precise, compliant with standards
LSM Testing Laboratory: 3D Microscopy and Surface Inspection
Using laser scanning microscopy (LSM), we measure surface structures, roughness, and topography in the micro- and submicrometer ranges. LSM enables three-dimensional visualization and non-contact analysis of coating systems, wear marks, cracks, and microstructures—ideal for quality assessment, damage analysis, and process optimization.
Laser scanning microscope (LSM) - Precise 3D surface analysis
The laser scanning microscope (LSM) in the encontec test laboratory enables non-contact 3D surface measurement with sub-nanometer resolution - ideal for sensitive, complex or high-precision components. The measurement is performed without sample movement, which minimizes distortions and measurement errors.

Typical use cases:
- 3D Visualization of Surfaces and Coating Systems
- Analysis of Cracks, Scratches, Wear, and Corrosion
- Evaluation of Roughness, Flatness, and Surface Height
- Investigation of Microstructures in Metals, Plastics, and Electronics
- Comparison of manufacturing parameters or material batches; fretting at contact points
Scope of Services:
- 3D Topographic Measurement Using Laser Scanning Microscopy
- Elevation profiles, roughness parameters, and surface characteristics
- Visualization of Layered Structures and Interfaces
- Can be combined with SEM/EDX or polished sample analysis
- Documentation of all relevant findings
Result:
- Precise 3D representation of surface topography
- Quantitative roughness and texture parameters
- Identification of defects, wear, or manufacturing deviations
- Comprehensive visual and measurement documentation
Technically precise 3D surface characterization
Confocal laser scanning microscopes capture the surface point by point or line by line in different focal positions. This creates a high-resolution 3D elevation model with high lateral and axial resolution.
In contrast to 2D profile measurements, area-based recording enables the reliable identification of local topographical structures.
Typical analyzable characteristics:
- Micro- and nanostructures
- 3D roughness parameters in accordance with relevant standards (e.g. ISO 25178)
- Pores, depressions and material inclusions
- Scoring, scratches and tribological marks
- Particles and local material irregularities
- Functional surfaces (plateaus, pockets, microchannels, lubricating film pockets)
Relevance of 3D roughness parameters in practice
Compared to 2D profile measurements, 3D roughness parameters provide significantly more comprehensive information on the functional behavior of a surface. They are crucial for the evaluation of:
- Friction and wear behavior
- Tightness and susceptibility to leaks
- Running-in behavior and lubricating film formation
- Load capacity and contact mechanics
- Microstructured functional surfaces (e.g. plain bearing surfaces, sealing surfaces)
This data supports the optimization of production processes, the monitoring of product quality and the analysis of error causes.
Technical advantages of the LSM at a glance
- Non-contact, non-destructive measurement - no mechanical influence on the surface
- Measurement without sample movement - ideal for sensitive or unstable components
- Sub-nanometer height resolution - precise detection of the finest structures
- Areal measurement data - complete 3D topography instead of one-dimensional profiles
- High repeatability due to stable optical scanning
- Fast data acquisition for efficient testing processes
- Comprehensive 3D evaluation software for topography, profiles and functional parameters
- Robust, low-maintenance system for continuous industrial use
Technical data
| Parameters | Specification |
| Measuring range | up to 100 mm diameter |
| Height resolution | up to 0.1 nm (axial) |
| Roughness measurement | Measurement of functional & standard-compliant 3D roughness parameters up to 19 nm |
| 3D evaluation | Area measurements, height profiles, volume & function parameters |
Typical areas of application
- 3D topography analyses of high-precision components
- Roughness measurement of sensitive or coated surfaces
- Quality assurance and final inspection
- Incoming goods and supplier qualification
- Research & Development
- Damage analysis (e.g. tribological traces, erosion or corrosion features)
- Analysis of metal, plastic, glass or hybrid materials
Added value for your projects
- Standard-compliant 3D surface measurement (e.g. in accordance with ISO 25178)
- High informative value thanks to complete surface models
- Precise, reproducible results in the nanometer range
- Comprehensible visualizations for test reports and presentations
- Technical support from experienced measurement technology experts
encontec - Your partner for reliable, standard-compliant 3D surface analysis
3D topography of a tool cutting edge - color-coded height map according to ISO 25178.
Macro image of a technical sealing surface to evaluate local surface features.
Laser scanning microscope in the test laboratory - non-contact 3D topography analysis.
Overview of services
What we measure
- 3D topographies and microstructures
- Standard-compliant 3D roughness parameters (ISO 25178)
- Pores, depressions, defects
- Scoring, scratches, tribological marks
- Functionally relevant microstructures (plateaus, pockets, microchannels)
Why it is relevant
3D measurement data provides crucial information about
- Wear & friction behavior
- Tightness & leakage
- Load capacity & contact mechanics
- Lubricating film formation & functional surfaces
Technical highlights
- Measuring range: up to 100 mm diameter
- Height resolution: up to 0.1 nm axial
- Roughness measurement: functional & standard-compliant parameters up to 19 nm
- Evaluation: 3D surfaces, profiles, volumes & functional characteristics
Areas of application
- Quality assurance & final inspection
- Research & Development
- Damage analysis
- Incoming goods inspection
- Measurement of metal, plastic, glass & coatings
Your advantages with encontec
- Precise, reproducible nanometer measurements
- Non-contact & non-destructive
- Meaningful 3D data instead of 2D profiles
- Ideal for sensitive or micro-structured surfaces
- Clear visualizations for reports & presentations